Failure mechanism and forming limit of tube axial compressive process
- 期刊名字:中国有色金属学会会刊(英文版)
- 文件大小:
- 论文作者:SUN Zhi-chao,YANG He
- 作者单位:School of Materials Science and Engineering
- 更新时间:2022-10-15
- 下载次数:次
Based on minimum energy principle for plastic forming,tearing and buckling failures mechanisms are explored and criteria for them are developed by theoretical analysis and experiment. Combined with finite element software developed forming limit and effects of process parameters on failures are investigated and proper parameters for stable forming are determined. The results show that: 1) The failures and forming limit are mainly determined by geometry and materials parameters of tube blank,fillet radius or half conical angle of die. For the process under fillet die,there exists a maximum fillet radius within which no tearing failure happens,and a maximum radius and a minimum radius range within which no buckling failure happens. For the process under conical die,there exists a maximum and minimum half conical angle range within which no tearing and buckling failures occur. 2) For both forming processes,the higher the value of material strain hardening exponent or the lower the value of relative thickness,the more impossible for tearing and buckling failures to occur,and the larger the ranges of fillet radius and half conical angle. The experiment results verify the reliability and practicability of this research.
-
C4烯烃制丙烯催化剂 2022-10-15
-
煤基聚乙醇酸技术进展 2022-10-15
-
生物质能的应用工程 2022-10-15
-
我国甲醇工业现状 2022-10-15
-
JB/T 11699-2013 高处作业吊篮安装、拆卸、使用技术规程 2022-10-15
-
石油化工设备腐蚀与防护参考书十本免费下载,绝版珍藏 2022-10-15
-
四喷嘴水煤浆气化炉工业应用情况简介 2022-10-15
-
Lurgi和ICI低压甲醇合成工艺比较 2022-10-15
-
甲醇制芳烃研究进展 2022-10-15
-
精甲醇及MTO级甲醇精馏工艺技术进展 2022-10-15