Valence variation of arsenic in bioleaching process of arsenic-bearing gold ore
- 期刊名字:中国有色金属学报(英文版)
- 文件大小:
- 论文作者:CUI Ri-cheng,YANG Hong-ying,CH
- 作者单位:School of Materials Science and Metallurgy
- 更新时间:2022-10-15
- 下载次数:次
The concentration and variational trend of As3+ and As5+, the bacterial resistance for the As3+ and As5+ and converting conditions from As3+ to As5+ were analyzed. The additive was used to prompt the bacterial leaching efficiency by changing valence state of arsenic. The results show that the concentration of As3+ is larger than that of As5+ in the lag phase. The concentration of As3+ decreases in the log phase, and is lower than that of As5+. HQ-0211 typed bacteria express better resistance for As3+ and As5+ and remain growing when the concentrations of As3+ and As5+ are above 6.0 g/L and 12.0 g/L, respectively. It is found that Fe3+ cannot oxidize As3+ singly as strong oxidant in the leaching system, but can cooperate with pyrite or chalcopyrite to do that. The oxidation of As3+ is prompted with addition of H2O2. The bacterial activity is improved in favor of bacterial leaching efficiency. NaClO restrains the bacterial growth to depress leaching efficiency because of the chloric compounds affecting bacterial activity.
-
C4烯烃制丙烯催化剂 2022-10-15
-
煤基聚乙醇酸技术进展 2022-10-15
-
生物质能的应用工程 2022-10-15
-
我国甲醇工业现状 2022-10-15
-
JB/T 11699-2013 高处作业吊篮安装、拆卸、使用技术规程 2022-10-15
-
石油化工设备腐蚀与防护参考书十本免费下载,绝版珍藏 2022-10-15
-
四喷嘴水煤浆气化炉工业应用情况简介 2022-10-15
-
Lurgi和ICI低压甲醇合成工艺比较 2022-10-15
-
甲醇制芳烃研究进展 2022-10-15
-
精甲醇及MTO级甲醇精馏工艺技术进展 2022-10-15