ASTM D790-2015 未增强和增强塑料及电绝缘材料挠曲性试验方法 Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials ASTM D790-2015 未增强和增强塑料及电绝缘材料挠曲性试验方法 Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials

ASTM D790-2015 未增强和增强塑料及电绝缘材料挠曲性试验方法 Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials

  • 标准类别:
  • 标准大小:
  • 标准编号:ASTM D790-2015
  • 标准状态:现行
  • 更新时间:2023-06-08
  • 下载次数:
标准简介

1.1 These test methods are used to determine the flexural properties of unreinforced and reinforced plastics, including highmodulus composites and electrical insulating materials utilizing a three-point loading system to apply a load to simply supported beam (specimen). The method is generally applicable to both rigid and semi-rigid materials, but flexural strength cannot be determined for those materials that do not break or that do not fail yield in the outer surface of the test specimen within the 5.0 % strain limit. 1.2 Test specimens of rectangular cross section are injection molded or, cut from molded or extruded sheets or plates, or cut from molded or extruded shapes. Specimens must be solid and uniformly rectangular. The specimen rests on two supports and is loaded by means of a loading nose midway between the supports. 1.3 Measure deflection in one of two ways; using crosshead position or a deflectometer. Please note that studies have shown that deflection data obtained with a deflectometer will differ from data obtained using crosshead position. The method of deflection measurement shall be reported. Note 1: Requirements for quality control in production environments are usually met by measuring deflection using crosshead position. However, more accurate measurement may be obtained by using an deflection indicator such as a deflectometer. Note 2: Materials that do not rupture by the maximum strain allowed under this test method may be more suited to a 4-point bend test. The basic difference between the two test methods is in the location of the maximum bending moment and maximum axial fiber stresses. The maximum axial fiber stresses occur on a line under the loading nose in 3-point bending and over the area between the loading noses in 4-point bending. A four-point loading system method can be found in Test Method D6272. 1.4 The values stated in SI units are to be regarded as the standard. The values provided i

标准截图
下一条:返回列表
版权:如无特殊注明,文章转载自网络,侵权请联系cnmhg168#163.com删除!文件均为网友上传,仅供研究和学习使用,务必24小时内删除。