New Evaluation on the Preoxidation Extent of Different PAN Precursors
- 期刊名字:材料科学技术学报
- 文件大小:
- 论文作者:Wangxi ZHANG,Jie LIU,Jieying L
- 作者单位:Department of Mechanical Engineering,Department of Carbon Fibers and Composites
- 更新时间:2023-04-15
- 下载次数:次
Structural changes in carbon fibers at each stage of, especially, preoxidation process are well known to play a great role in achieving the ultimate product quality. Differential scanning calorimetry (DSC), scanning electron microscope (SEM), density method and optical microscope were used to characterize the preoxidation extent. A conventional pproach, e.g., density aim, to evaluate the extent of preoxidation is not very exact. A DSC curve of a PAN precursor only can provide general information, major in the temperature regime of preoxidation reaction. However,the evaluation of a preoxidation extent, especially from conventional preoxidation temperature with a great span egime of 200~400℃, is put forward in this paper, in which the evolution of core/shell morphological structure is a kind of straightforward evidence.
-
C4烯烃制丙烯催化剂 2023-04-15
-
煤基聚乙醇酸技术进展 2023-04-15
-
生物质能的应用工程 2023-04-15
-
我国甲醇工业现状 2023-04-15
-
JB/T 11699-2013 高处作业吊篮安装、拆卸、使用技术规程 2023-04-15
-
石油化工设备腐蚀与防护参考书十本免费下载,绝版珍藏 2023-04-15
-
四喷嘴水煤浆气化炉工业应用情况简介 2023-04-15
-
Lurgi和ICI低压甲醇合成工艺比较 2023-04-15
-
甲醇制芳烃研究进展 2023-04-15
-
精甲醇及MTO级甲醇精馏工艺技术进展 2023-04-15